1, safe and environmentally friendly, non-toxic no pollution;
2, the basic level of shrinkage and deformation cracking adaptability;
3, film strength, high elongation;
4, It can be directly on the wet base construction, high bond strength;
5, cold construction, easy operation, short construction period.
															 
														
								GB/T23445-2009《Polymer-modified cement compounds for waterproofing membrane》
Serial number  | Item  | Performance  | 
Ⅰ  | Ⅱ  | Ⅲ  | 
1  | solid content/% ≥  | 70  | 70  | 70  | 
2  | Tensile strength  | No treatment/MPa ≥  | 1.2
   | 1.8
   | 1.8
   | 
heat treatment/% ≥  | 80  | 80  | 80  | 
alkali treatment/% ≥  | 60  | 70  | 70  | 
immersing in water/% ≥  | 60  | 70  | 70  | 
UV treatment/% ≥  | 80  | -  | -  | 
3  | Retention
tensile 
strength  | No treatment≥  | 200
   | 80
   | 30
   | 
heat treatment ≥  | 150  | 65  | 20  | 
alkali treatment ≥  | 150  | 65  | 20  | 
immersing in water ≥  | 150  | 65  | 20  | 
UV treatment ≥  | 150  | -  | -  | 
4  | Cold bending(φ10mmstick)  | -10℃flawless  | 450  | 250  | 
5  | Bonding strength/MPa  | No treatment≥  | 0.5
   | 0.7
   | 1.0
   | 
Wet treatment ≥  | 0.5  | 0.7  | 1.0  | 
alkali treatment ≥  | 0.5  | 0.7  | 1.0  | 
immersing in water ≥  | 0.5  | 0.7  | 1.0  | 
6  | waterproofness(0.3MPa,30min)  | waterproof  | waterproof  | waterproof  | 
7  | anti-permeability(back side)/MPa ≥  | -  | 0.6  | 0.8  |